ECOCRETE™ Twisted Bundle PP Fiber

High-performance crack control and toughness for concrete, shotcrete, and precast.

What is Twisted Bundle PP Fiber?

Twisted Bundle PP Fiber (also called bundled PP macro fiber) is produced by precision drawing and surface treatment so that each bundle separates rapidly during mixing and forms a dense 3D reinforcement network. Compared with plain monofilament, the twisted bundle delivers faster opening, stronger mechanical anchorage and higher efficiency at the same dosage. It is chemically inert, non-corrosive, lightweight, and causes zero wear to mixers and pumps.

ECOCRETE™ Twisted Bundle PP Fiber is engineered from premium polypropylene and processed to open quickly in mixing, dispersing into thousands of micro-filaments that bridge micro-cracks and toughen the matrix. It improves crack control, anti-seepage, impact resistance and durability across floors, roads, tunnels and water structures.

Twisted bundle polypropylene macrofiber for concrete reinforcement

Technical Parameter

  • Material: Virgin Polypropylene (PP)
  • Form: Twisted Bundle (macro)
  • Density: 0.91 g/cm³
  • Equivalent Diameter: 0.60 ± 0.05 mm
  • Length Options: 40 / 50 / 56 mm (custom lengths available)
  • Tensile Strength: ≥ 450 MPa
  • Elastic Modulus: ≥ 5,500 MPa
  • Elongation at Break: 20 ± 5%
  • Alkali/Acid Resistance: ≥ 95% retention
  • Melting Point: 160–170 °C
  • Water Absorption: None
Twisted bundle polypropylene macrofiber for concrete reinforcement
Twisted Bundle PP Fiber laid in slab before concrete casting

Key Benefits of Twisted Bundle PP Fiber

  1. Crack Control: Bridges micro-cracks during plastic and drying shrinkage; reduces crack width and density.
  2. Anti-Seepage & Durability: Lowers connected porosity for better water-tightness, freeze–thaw and chloride resistance.
  3. Toughness & Impact: Increases post-crack load capacity, flexural strength, impact and fatigue resistance.
  4. Chemical & Corrosion Proof: Non-rusting, non-conductive, excellent resistance to salts, alkali and acids.
  5. Easy Mixing: Rapid opening from bundle to filaments; uniform dispersion; no balling; no equipment abrasion.
  6. Cost-Efficient Alternative: Reduces risk of surface cracking and maintenance; can replace part of secondary steel mesh in many applications.
Twisted Bundle PP Fiber for precast concrete wall panels under gantry crane

Applications of Twisted Bundle PP Fiber

  1. Industrial Floors & Pavements: warehouses, logistics hubs, cold rooms, sports courts
  2. Roads & Bridges: pavements, parapets, barriers, overlays
  3. Shotcrete: tunnels, mines, slope stabilization, culverts
  4. Water & Municipal Works: dams, tanks, canals, water-retaining and anti-seepage structures
  5. Precast Elements: pipes, panels, manholes, modular components
  6. Marine & Chemical Environments: coastal works, chemical plants, corrosion-prone areas
Twisted Bundle PP Fiber for precast concrete wall panels under gantry crane
Worker handling bagged AR-glass fibers in front of stacked inventory

How to Use & Recommended Dosage

  • Typical Dosage (general crack control): 1.0–1.5 kg/m³
  • Enhanced Toughness / Shotcrete: 3.0–6.0 kg/m³
  • Hybrid Recommendation: For surface crack control on slabs, combine Twisted Bundle PP Fiber 1.0 kg/m³ with PP Mesh/Monofilament 0.4–0.6 kg/m³ for optimized micro- and macro-crack bridging.
  • Mixing Procedure: Add aggregates → add Twisted Bundle PP Fiber → add cement → add water/admixtures → mix until full dispersion; adjust water or admixture for target workability.
  • Compatibility: Works with standard ready-mix, pumping and shotcreting equipment; compatible with common admixtures.

Packaging & Logistics

Inner Packs: 1–3 kg PE bags (easy dose)

Outer Packs: 10–20 kg woven bag or carton

Palletization: ~400 kg/pallet (customizable)

20′HC (palletized): approx. 7.6 tons · 40′HC: approx. 17.6 tons
Each shipment includes packing list and QC documents to speed up customs clearance.

Why Ecocrete™

  • Factory Direct: In-house lines and strict QC for consistent supply and stable lead time.
  • Proven in Projects: Floors, tunnels, waterworks and precast plants worldwide.
  • Fast Dispersion Technology: Bundles open quickly into dense filament networks.
  • Complete Paperwork: COA / SDS / TDS, ISO 9001 and project random inspections available.
  • Global Support: Technical advice and shipping options for distributors and contractors.
PP fiber extrusion lines forming consistent monofilament
Palletized fiber bags stored in a covered warehouse

FAQs — Twisted Bundle PP Fiber

Certificates & Test Reports

Every batch is traceable. We provide COA, SDS, TDS, factory ISO9001 and project-specific third-party test reports upon request. Original stamped copies and bilingual versions are available.

Send message

Let's make a difference

Tell us about your project and timeline. We’ll reply with factory pricing and a shipping plan.

Schedule Appointment

Fill out the form below, and we will be in touch shortly.

Contact Information

Schedule Appointment

Fill out the form below, and we will be in touch shortly.

Contact Information

Schedule Appointment

Fill out the form below, and we will be in touch shortly.

Contact Information