100% inorganic, alkali-resistant reinforcement for longer-lasting concrete and GRC.

Alkali Resistant Glass Fiber (AR glass) is a 100% inorganic fiber engineered for cementitious environments. It offers excellent alkali resistance, strong interfacial grip, high elastic modulus, and very high tensile/bending/impact strength, with non-flammability, frost resistance and robust anti-crack/anti-seepage performance. It is easy to mold and design into thin, light yet strong components for modern construction.
ECOCRETE™ Alkali Resistant Glass Fiber is a high-modulus, non-flammable, alkali-stable reinforcement for concrete and mortar. It provides strong bonding, excellent crack control and water-tightness, while resisting temperature and humidity swings—ideal for precast panels, GRC/GFRC, tunnels, waterworks and durable repair systems.
Mixing: Add aggregates → dose Alkali Resistant Glass Fiber → add cement → add water/admixtures; mix to full dispersion. Maintain target workability with proper water-reducing agents. (Good pumpability reported.)
Design Notes: Select length by section thickness and placement method (12/20 mm for thin sections and finishes; 36 mm for deeper crack-bridging). Conduct a trial mix to confirm workability and finishing with your local materials.
We work with reliable forwarders to offer FCL/LCL solutions worldwide. Consolidation options, pallet planning and complete QC paperwork help streamline customs and shorten lead time.
A: AR glass contains zirconia (ZrO₂ 16.7%) for alkali durability in cement, maintaining strength/modulus over time.
A: Yes—its high modulus and strong bonding enhance crack resistance and anti-seepage performance.
A: Yes—AR glass is non-flammable and stable under temperature/humidity variations; frost-resistant.
A: Use 12–20 mm for thin sections and surface finishing; 36 mm for deeper crack-bridging. Trial mixes are recommended.
A: The fiber mixes uniformly with low water demand and shows good pumpability when correctly dispersed.
Tell us about your project and timeline—we’ll reply with factory pricing and a shipping plan tailored to your country and port.
Fill out the form below, and we will be in touch shortly.
Fill out the form below, and we will be in touch shortly.
Fill out the form below, and we will be in touch shortly.