ECOCRETE™ Mesh Polypropylene Fiber

Micro-mesh crack control for durable, watertight, and tougher concrete.

What is Mesh Polypropylene Fiber?

Mesh Polypropylene Fiber is a concrete reinforcement fiber made from virgin PP. Its filaments are inter-connected in a mesh structure that separates rapidly under mixing shear, creating countless micro-bridges to control plastic and drying shrinkage, enhance fatigue resistance, and increase tensile performance—without corroding or wearing equipment.

ECOCRETE™ Mesh Polypropylene Fiber (PP mesh fiber) opens into a dense, three-dimensional mesh during mixing, bridging micro-cracks and improving crack control, toughness, and water-tightness. Ideal for industrial floors, pavements, tunnels, waterworks and precast elements.

Laboratory weight check of Mesh Polypropylene Fiber specimens

Technical Parameter

  • Material: Polypropylene (PP)
  • Form: Mesh / bundled mesh (macro-mesh)
  • Density: 0.91 g/cm³
  • Equivalent Diameter: ≈100 μm
  • Length Options: 19–60 mm (customizable)
  • Tensile Strength: ≥460 MPa
  • Elastic Modulus: ≥4800 MPa
  • Elongation at Break: 20 ± 5%
  • Melting Point: 160–170 °C
  • Acid/Alkali Resistance: ≥95% retention
  • Water Absorption: None
Laboratory weight check of Mesh Polypropylene Fiber specimens
Concrete surface before vs after crack control with AR glass fibers

Key Benefits of Mesh Polypropylene Fiber

  1. Crack Control: Reduces plastic and drying shrinkage cracking; lowers crack width and density.
  2. Durability & Anti-Seepage: Improves water-tightness; resists chemicals and corrosion.
  3. Toughness & Fatigue: Enhances post-crack behavior, impact and fatigue resistance.
  4. Fast Dispersion & Easy Mixing: Mesh opens quickly into many filaments; uniform distribution, no balling.
  5. Lightweight & Non-Conductive: No rusting; friendly to pumps and mixers.
Mesh Polypropylene Fiber for airport apron concrete

Applications of Mesh Polypropylene Fiber

  1. Industrial floors & pavements: warehouses, bridge decks, airport aprons, factory slabs
  2. Tunnels & mining: linings, walls, crown/roof shotcrete (reduced rebound)
  3. Water & municipal works: channels, dams, tanks, anti-seepage structures
  4. Precast components: pipes, panels, manholes, modular parts
  5. Sports grounds & landscaping bases
Mesh Polypropylene Fiber for airport apron concrete
Worker handling bagged AR-glass fibers in front of stacked inventory

How to Use & Recommended Dosage

  • Typical crack control in slabs/mortar: 0.6–1.5 kg/m³ (micro-mesh)
  • High crack-control / surface finish: up to 2.0 kg/m³ depending on spec
  • Hybrid strategy (for slabs): Combine Mesh Polypropylene Fiber 0.4–0.6 kg/m³ with Twisted Bundle PP Fiber 1.0–1.5 kg/m³ to bridge both micro- and macro-cracks efficiently.
  • Mixing order: Aggregates → fiber → cement → water/admixture → mix to full dispersion; adjust water/superplasticizer to target slump.

Packaging & Logistics

Inner packs: 1–3 kg PE bags

Outer packs: 10–20 kg woven bag or carton

Palletization: ≈500 kg/pallet (customizable)

20′ container (palletized): ≈8 tons, 10 pallets (0.8 t/pallet)

40′ HQ (palletized): ≈20 tons, 20 pallets (1.0 t/pallet)

Lead time: 5–10 days depending on order mix

Why Ecocrete™

  • Factory Direct: In-house lines and QC ensure consistent supply and stable lead time.
  • Proven Performance: Used in roads, tunnels, water projects and precast plants.
  • Fast-Opening Mesh: Designed for rapid dispersion and uniform distribution.
  • Complete Paperwork: COA / SDS / TDS, ISO 9001 and project inspection reports available.
  • Flexible Packaging: Inner bag sizes and pallets tailored to your site workflow.
PP fiber extrusion lines forming consistent monofilament
Palletized fiber bags stored in a covered warehouse

FAQs — Mesh Polypropylene Fiber

Certificates & Test Reports

Every batch is traceable. We provide COA, SDS, TDS, factory ISO9001 and project-specific third-party test reports upon request. Original stamped copies and bilingual versions are available.

Send message

Let's make a difference

Share your project details and timeline—our team will revert with factory pricing and a shipping plan tailored to your country and port.

Schedule Appointment

Fill out the form below, and we will be in touch shortly.

Contact Information

Schedule Appointment

Fill out the form below, and we will be in touch shortly.

Contact Information

Schedule Appointment

Fill out the form below, and we will be in touch shortly.

Contact Information