Ecocrete™ PP Monofilament Fiber

PP Monofilament Fiber

PP monofilament fibers act as secondary reinforcement in concrete/mortar. They limit plastic/drying/thermal shrinkage cracks, improve impermeability, abrasion resistance and toughness, extending service life—ideal for industrial floors, precast, shotcrete and general construction.

Lab tensile/adhesion testing of AR glass fibers and cement matrix

Technical Parameter

Density: 0.91 g/cm³
Shape: Monofilament
Equivalent Diameter: 18–50 μm
Acid-base Resistance: ≥95%
Fiber Length: 0.5 mm, 3 mm, 4 mm, 6 mm, 8 mm, 9 mm, 12 mm, 19 mm, customizable
Tensile Strength: ≥500 MPa
Melting Point: 160–170 ℃
Elastic Modulus: ≥4000 MPa
Elongation at Break: 25 ± 5%
Water Absorption: Non-absorbent-

Lab tensile/adhesion testing of AR glass fibers and cement matrix
Concrete surface before vs after crack control with AR glass fibers

Key Benefits

  1. Controls plastic/drying/thermal shrinkage cracking; boosts impermeability & abrasion resistance.
  2. High acid/alkali resistance; non-absorbent.
  3. Ultra-fine options (e.g., 18 μm/22 μm); good dispersion with antistatic finish; high purity PP pellets.
  4. Flexible packaging, private-label available.

Applications

  • Highways & pavements, bridge decks, airport runways, industrial floors
  • Tunnels/shotcrete & mining
  • Rivers/dams/reservoirs
  • Defense & marine works
  • Precast pipes/slabs/boards
  • Pumpable/shotcrete
  • Chemical plants (alkali/chemical resistance), UHPC, cement & mortar
Worker handling bagged AR-glass fibers in front of stacked inventory

Packaging & Logistics

  • Inner bags: 0.6–2 kg;Outer: 20–25 kg woven/box;Pallet: 500 kg;custom available.

  • Container load: 20’GP ≈ 10 t (1 t/pallet × 10);40’HQ ≈ 24 t (1.2 t/pallet × 20)。Lead time 5–10 days.

Ecocrete™ PP Monofilament Fiber​

SHIPMENT

Global Shipping & Delivery

We ship worldwide with export-ready packing and documentation. Each shipment is photographed and recorded for traceability—so you know exactly what you receive.

Why Ecocrete™

  • Ultra-fine & high-purity PP; excellent dispersion with antistatic oiling.
  • Process strength:heated-axis drawing & spinneret tech for finer filaments(min 18 μm)。
  • Custom lengths & packing to fit job-site workflow.
PP fiber extrusion lines forming consistent monofilament
Palletized fiber bags stored in a covered warehouse

FAQs

When should I choose between PP mesh fiber and PP macro fiber?

Monofilament is more suitable for concrete or mortars requiring high crack resistance, impermeability, and surface quality. For higher toughness and load-bearing properties, consider PP macro or steel fibers (links to related products on this site). Reference: PP mesh fiber and macro fiber introduction and dosage range.

Follow the order of “aggregate → fiber → cement → water → mixing → adding water” to ensure complete dispersion. Asphalt should be sprayed after dry mixing for 20 seconds.

Inner and outer bags and pallets are customizable, and private labeling and documentation are supported.

Certificates & Test Reports

Every batch is traceable. We provide COA, SDS, TDS, factory ISO9001 and project-specific third-party test reports upon request. Original stamped copies and bilingual versions are available.

Technical Data Sheet (TDS) for AR glass fiber

TDS — Technical Data Sheet

ISO 9001 quality management certificate

ISO 9001 — Quality Management

Project random inspection report

Project Random Inspection

COA – Certificate of Analysis (AR-glass batch)

COA — Certificate of Analysis

Safety Data Sheet (SDS) for AR glass fiber

SDS — Safety Data Sheet

Send message

Let's make a difference

We’re here to help you find the right fiber solution.
Leave us a message and let’s make your project stronger together.

Schedule Appointment

Fill out the form below, and we will be in touch shortly.

Contact Information

Schedule Appointment

Fill out the form below, and we will be in touch shortly.

Contact Information

Schedule Appointment

Fill out the form below, and we will be in touch shortly.

Contact Information