PP monofilament fibers act as secondary reinforcement in concrete/mortar. They limit plastic/drying/thermal shrinkage cracks, improve impermeability, abrasion resistance and toughness, extending service life—ideal for industrial floors, precast, shotcrete and general construction.
Density: 0.91 g/cm³
Shape: Monofilament
Equivalent Diameter: 18–50 μm
Acid-base Resistance: ≥95%
Fiber Length: 0.5 mm, 3 mm, 4 mm, 6 mm, 8 mm, 9 mm, 12 mm, 19 mm, customizable
Tensile Strength: ≥500 MPa
Melting Point: 160–170 ℃
Elastic Modulus: ≥4000 MPa
Elongation at Break: 25 ± 5%
Water Absorption: Non-absorbent-
Inner bags: 0.6–2 kg;Outer: 20–25 kg woven/box;Pallet: 500 kg;custom available.
Container load: 20’GP ≈ 10 t (1 t/pallet × 10);40’HQ ≈ 24 t (1.2 t/pallet × 20)。Lead time 5–10 days.
We ship worldwide with export-ready packing and documentation. Each shipment is photographed and recorded for traceability—so you know exactly what you receive.
Monofilament is more suitable for concrete or mortars requiring high crack resistance, impermeability, and surface quality. For higher toughness and load-bearing properties, consider PP macro or steel fibers (links to related products on this site). Reference: PP mesh fiber and macro fiber introduction and dosage range.
Follow the order of “aggregate → fiber → cement → water → mixing → adding water” to ensure complete dispersion. Asphalt should be sprayed after dry mixing for 20 seconds.
Inner and outer bags and pallets are customizable, and private labeling and documentation are supported.
We’re here to help you find the right fiber solution.
Leave us a message and let’s make your project stronger together.
Fill out the form below, and we will be in touch shortly.
Fill out the form below, and we will be in touch shortly.
Fill out the form below, and we will be in touch shortly.