Row-bonded, water-soluble glued steel fibers for fast dosing, clean dispersion and high toughness.

Glued Steel Fiber (also called “row-bonded steel fiber”) uses a high-strength, low-carbon steel wire base. Fibers are glued in strips/rows for easy handling and dosing; once inside the mixer, water dissolves the glue so fibers spread into a dense 3D network. Compared with loose bulk fibers, glued fibers feed cleaner, clump less, and disperse faster—ideal for high-efficiency slabs and heavy-duty structures.
ECOCRETE™ Glued Steel Fiber is cold-drawn high-tensile wire cut to length and bonded into rows with a water-soluble glue. During mixing, the glue dissolves and the fibers release rapidly, achieving uniform dispersion without balling. The result is tighter crack control and superior post-crack load capacity for floors, pavements, precast and tunnels.
Models & Core Specs (examples):
Notes: Custom lengths and aspect ratios available to match design targets (residual strength, joint spacing, slab thickness).
Mixing sequence (cementitious): Aggregates → Glued Steel Fiber (dose the rows gradually) → cement → water + admixtures → mix to full dispersion (glue dissolves) → finish as usual.
Design note: Fibers do not replace primary reinforcement where required; follow the engineer’s design and local codes.
We work with reliable forwarders for FCL/LCL worldwide. Consolidation options, pallet planning and complete QC paperwork help streamline customs and shorten lead time.
A: Glued rows dose faster and cleaner; the water-soluble glue dissolves in the mixer so fibers separate thoroughly, reducing clumping risk.
A: The glue is designed to not affect concrete strength once dissolved; adjust superplasticizer to maintain slump/flow if needed.
A: Choose by slab thickness, joint spacing and target residual strength. 30–35 mm for thinner toppings/repairs; 50–60 mm for industrial floors and bridge decks.
A: In many crack-control specs it can reduce or replace secondary mesh—subject to structural design. Primary load-bearing reinforcement must follow code.
A: 20 kg per carton/bag; 1.5–2.0 t per pallet; ≈24 t per 40′ HQ (12 pallets × 2 t). Lead time 5–10 days.
Tell us your project and schedule—we’ll reply with factory pricing and a shipping plan tailored to your country and port.
Fill out the form below, and we will be in touch shortly.
Fill out the form below, and we will be in touch shortly.
Fill out the form below, and we will be in touch shortly.