Karbon Fiberli Beton Hazırlama ve Karışım Tasarımı Kılavuzu

Carbon fiber can give a cement-based mixture a useful combination of crack bridging, low fiber weight, and electrical conductivity. It also creates a demanding production problem: fine, chopped filaments tend to cling together. A strong fiber on a data sheet will do little for a concrete element if most of the filaments remain in bundles. […]