Ultra-high strength micro-reinforcement for crack control, toughness and fatigue life.

Micro Copper Coated Steel Fiber is a high-performance steel micro-fiber whose copper-plated surface enhances corrosion resistance and interfacial bond. Available as straight cut or hooked-end types, the fibers form a dense 3-D reinforcement network in concrete, reducing crack width/density and upgrading post-crack load-carrying capacity. Compared with secondary mesh, dosing is fast and placement is unchanged—ideal for high-efficiency slabs and UHPC components.
ECOCRETE™ Micro Copper Coated Steel Fiber is manufactured from ultra-fine steel wire with a copper coating, then precision cut into straight or hooked fibers. It disperses rapidly, bonds strongly with cement paste and dramatically improves tensile/flexural capacity, impact resistance and fatigue durability in floors, pavements, precast and repair systems.
Mixing sequence (cementitious): Aggregates → Micro Copper Coated Steel Fiber (dose gradually) → cement → water + admixtures → mix to full dispersion; adjust superplasticizer to maintain workability.
Design note: Fiber does not replace primary reinforcement where required. Follow the structural engineer’s design and local codes.
We partner with reliable forwarders for FCL/LCL worldwide. Consolidation options, pallet planning and full QC documentation help streamline customs and shorten lead time.
A: Straight improves finish and pumpability at lower dosages; hooked increases pull-out resistance and post-crack toughness. Select by slab thickness, joint spacing and load.
A: In many crack-control applications, it can reduce or replace secondary mesh—subject to the engineer’s design. Primary load-bearing reinforcement must follow code.
A: Expect some slump reduction. Use proper mixing time and superplasticizer to maintain target workability; finish with conventional equipment or laser screeds.
A: The copper layer helps protect the steel surface and enhances bond. Good concrete cover and mix design are still essential for durability.
A: We supply COA / SDS / TDS with each batch and support on-site trials upon request.
Tell us your project and schedule—we’ll reply with factory pricing and a shipping plan tailored to your country and port.
Fill out the form below, and we will be in touch shortly.
Fill out the form below, and we will be in touch shortly.
Fill out the form below, and we will be in touch shortly.